” Bombs charged with granular UF4 and finely divided Mg (the latter in excess) are heated to 500 to 700 °C (930 to 1,300 °F), at which point an exothermic (heat-producing) reaction occurs. The heat of reaction is sufficient to liquefy the conversion contents of the…