At what temperatures can cobalt-containing superalloys operate?

Created from Britannica articles using AI. AI can make mistakes, so verify using Britannica articles.

Cobalt-containing superalloys are engineered to maintain their structural integrity and strength under extreme conditions, such as those found in jet engines and gas turbines. These specialized alloys are capable of operating at temperatures reaching up to 1,150 °C (2,100 °F).1

By incorporating cobalt into these materials, manufacturers significantly enhance the high-temperature strength and corrosion resistance of alloys based on metals like nickel and chromium. While standard high-temperature steel alloys typically retain their strength above 650 °C (1,200 °F), the development of superalloys has allowed for the even higher operating temperatures required in modern turbine technology.21